Wheel Materials vs. Chemical Compatibility Guide
Casters and Wheels need to operate in a wide range of environments. Chemical exposure can greatly reduce the lifespan of certain materials so it's essential to pick the right wheel materials as compared to the chemical environments those wheels will be exposed to. Use our guide to see what wheels best fit your application. As always if you have any questions give us a call or contact us.
Wheel Materials vs. Chemical Compatibility Guide
Casters and Wheels need to operate in a wide range of environments. Chemical exposure can greatly reduce the lifespan of certain materials so it's essential to pick the right wheel materials as compared to the chemical environments those wheels will be exposed to. Use our guide to see what wheels best fit your application. As always if you have any questions give us a call or contact us.
Chlorine, Dry
Cl₂
Chlorine Dry Caster Compatibility
Chemical Overview
Molecular Formula: Cl₂
Physical Properties: Chlorine (dry) is a greenish-yellow gas with a pungent odor. It has a density of 3.21 g/L at 0°C and is highly reactive and corrosive, especially to metals. (Source: PubChem)
Industrial Applications
Dry chlorine is used in water treatment, chemical synthesis, and bleaching processes. Caster wheels may be exposed in chemical plants or storage areas handling chlorine gas.
Wheel Material Compatibility Summary
Best Suited (A/B): Polyolefin, Nylon Glass Filled, and Polyurethane on Aluminum Core are highly resistant to dry chlorine.
Avoid (C/D): Avoid Ductile Cast Iron, Forged Steel, and V-Grooved Iron due to severe corrosion risks.
Wheel Compatibility Table
| Wheel Material | Interaction Description | Rating |
|---|---|---|
| Ductile Cast Iron | Highly corrosive; rapid degradation. | D |
| Elastomer | Moderate resistance; some degradation possible. | C |
| Forged Steel | Corrodes rapidly; unsuitable. | D |
| Neoprene/Nylon Glass Core | Neoprene degrades; nylon core resists but overall poor. | C |
| Nylon | Good resistance; minimal degradation. | B |
| Nylon Glass Filled | Excellent resistance; highly stable. | A |
| Phenolic | Good resistance; slight degradation possible. | B |
| Polyolefin | Excellent chemical inertness. | A |
| Polyurethane on Aluminum Core | Good resistance; aluminum unaffected. | A |
| Polyurethane on Iron Core | Polyurethane resists; iron core corrodes. | C |
| Rubber | Degrades; unsuitable for chlorine exposure. | D |
| Solid Elastomer | Moderate degradation; limited suitability. | C |
| Thermoplastic Rubber | Degrades; poor performance. | D |
| Urethane | Good resistance; slight degradation possible. | B |
| V-Grooved Iron | Corrodes rapidly; unsuitable. | D |
Conclusion
Dry chlorine is highly corrosive, and Polyolefin, Nylon Glass Filled, and Polyurethane on Aluminum Core are the best choices. Avoid metal-based wheels like Ductile Cast Iron and Rubber due to corrosion and degradation. For further guidance, contact us at CasterTech.