Wheel Materials vs. Chemical Compatibility Guide
Casters and Wheels need to operate in a wide range of environments. Chemical exposure can greatly reduce the lifespan of certain materials so it's essential to pick the right wheel materials as compared to the chemical environments those wheels will be exposed to. Use our guide to see what wheels best fit your application. As always if you have any questions give us a call or contact us.
Wheel Materials vs. Chemical Compatibility Guide
Casters and Wheels need to operate in a wide range of environments. Chemical exposure can greatly reduce the lifespan of certain materials so it's essential to pick the right wheel materials as compared to the chemical environments those wheels will be exposed to. Use our guide to see what wheels best fit your application. As always if you have any questions give us a call or contact us.
Formaldehyde (40%)
CH₂O
Formaldehyde 40% Caster Compatibility
Chemical Overview
Molecular Formula: CH₂O
Physical Properties: Formaldehyde (40% aqueous solution, formalin) is a colorless liquid with a pungent odor. It has a density of ~1.08 g/cm³, a boiling point of ~100°C, and is miscible with water. It is toxic and mildly acidic. (Source: PubChem)
Industrial Applications
Formaldehyde is used in resins, disinfectants, and as a preservative. Caster wheels may be exposed in laboratories, medical facilities, or manufacturing plants.
Wheel Material Compatibility Summary
Best Suited (A/B): Polyolefin, Nylon Glass Filled, and Polyurethane on Aluminum Core are highly resistant to formaldehyde 40%.
Avoid (C/D): Avoid Ductile Cast Iron, V-Grooved Iron, and Rubber due to potential corrosion or degradation.
Wheel Compatibility Table
| Wheel Material | Interaction Description | Rating |
|---|---|---|
| Ductile Cast Iron | Mild corrosion possible; not ideal. | C |
| Elastomer | Good resistance; minimal effect. | B |
| Forged Steel | Mild corrosion risk; generally resistant. | B |
| Neoprene/Nylon Glass Core | Neoprene resists; nylon core stable. | B |
| Nylon | Excellent resistance; chemically stable. | A |
| Nylon Glass Filled | Highly resistant; no degradation. | A |
| Phenolic | Good resistance; slight absorption possible. | B |
| Polyolefin | Excellent chemical inertness. | A |
| Polyurethane on Aluminum Core | Highly resistant; aluminum unaffected. | A |
| Polyurethane on Iron Core | Polyurethane resists; iron core may corrode slightly. | B |
| Rubber | Moderate degradation; unsuitable for prolonged exposure. | C |
| Solid Elastomer | Good resistance; minimal effect. | B |
| Thermoplastic Rubber | Moderate degradation; some softening. | C |
| Urethane | Good resistance; chemically stable. | B |
| V-Grooved Iron | Mild corrosion possible; not ideal. | C |
Conclusion
Formaldehyde 40% is mildly acidic, and Polyolefin, Nylon Glass Filled, and Polyurethane on Aluminum Core are ideal choices. Avoid Ductile Cast Iron and Rubber for prolonged exposure due to corrosion or degradation risks. For more information, contact us at CasterTech.