Wheel Materials vs. Chemical Compatibility Guide
Casters and Wheels need to operate in a wide range of environments. Chemical exposure can greatly reduce the lifespan of certain materials so it's essential to pick the right wheel materials as compared to the chemical environments those wheels will be exposed to. Use our guide to see what wheels best fit your application. As always if you have any questions give us a call or contact us.
Wheel Materials vs. Chemical Compatibility Guide
Casters and Wheels need to operate in a wide range of environments. Chemical exposure can greatly reduce the lifespan of certain materials so it's essential to pick the right wheel materials as compared to the chemical environments those wheels will be exposed to. Use our guide to see what wheels best fit your application. As always if you have any questions give us a call or contact us.
Tannic Acid
C₇₆H₅₂O₄₆
Tannic Acid Caster Compatibility
Chemical Overview
Molecular Formula: C₇₆H₅₂O₄₆ (approximate)
Physical Properties: Tannic acid is a yellowish to light brown amorphous powder or granules, soluble in water (1 g/0.35 mL at 20°C). It has a weak acidic pH (~3-4 in solution) and a density of ~0.4 g/cm³ (bulk). It is non-corrosive but can stain materials. (Source: PubChem)
Industrial Applications
Tannic acid is used in:
- Leather Tanning: To convert hides into leather.
- Textile Dyeing: As a mordant for dyes.
- Pharmaceuticals: In astringents and antiseptics.
- Exposure Scenarios: Spills in tanning or textile facilities may contact caster wheels.
Wheel Material Compatibility Summary
Best Suited Materials (A/B Ratings): Polyolefin, Nylon, and Phenolic (A) resist weak acids. Most materials (B) show minimal interaction due to low corrosivity.
Materials to Avoid (C/D Ratings): None; tannic acid is mildly acidic and generally safe for most wheel materials.
Wheel Compatibility Table
| Wheel Material | Interaction Description | Rating |
|---|---|---|
| Ductile Cast Iron | Minimal corrosion; possible staining. | B |
| Elastomer | Resistant to weak acids; no degradation. | A |
| Forged Steel | Minimal corrosion; possible staining. | B |
| Neoprene/Nylon Glass Core | Both resist weak acids; unaffected. | A |
| Nylon | Excellent resistance to weak acids. | A |
| Nylon Glass Filled | Similar to nylon; highly resistant. | A |
| Phenolic | Resistant to weak acids; unaffected. | A |
| Polyolefin | Excellent inertness; unaffected. | A |
| Polyurethane on Aluminum Core | Polyurethane and aluminum resist weak acids. | A |
| Polyurethane on Iron Core | Polyurethane resists; iron minimally affected. | B |
| Rubber | Resistant to weak acids; minimal impact. | A |
| Solid Elastomer | Resistant to weak acids. | A |
| Thermoplastic Rubber | Resistant to weak acids. | A |
| Urethane | Resistant to weak acids; minimal impact. | A |
| V-Grooved Iron | Minimal corrosion; possible staining. | B |
Conclusion
Tannic acid’s mild acidity makes Polyolefin, Nylon, and Phenolic wheels (A ratings) excellent choices. Most materials perform well (B ratings) with minimal risk of corrosion. For assistance, contact CasterTech.